No.1, 2   3 Liquid Flux, Fumeless Flux, Flux for C.G.L   Flux for Wire Materials

No.1, 2 3 Liquid Flux, Fumeless Flux, Flux for C.G.L Flux for Wire Materials


Negotiable Min Order Quantity Unit

Required Quantity
Place of Origin
Payment Terms
Negotiable
Production method
Negotiable
Shipping / Lead Time
Negotiable / Negotiable
Keyword
Category
Other Chemicals

KB ENG

Country / Year Established
South Korea South Korea /
Business type
Others
Verified Certificate

16

DUNS

Product name No.1, 2 3 Liquid Flux, Fumeless Flux, Flux for C.G.L Flux for Wire Materials Certification -
Category Other Chemicals Ingredients -
Keyword - Unit Size -
Brand name - Unit Weigh -
origin Stock -
Supply type - HS code -

Product Information

In order to get excellent plated ware with melting zinc-galvanizing, we, first of all, should treat the ware carefully before the galvanization. For which, we should remove impurities completely on the surface of the material to make it clean. We can not expect good results because an invisible film is created during washing or drying after cleaning with hydrochloric acid or sulfuric acid and an oxide film is again created on the surface of the zinc bath. So, we can get good plated ware only by using proper flux to remove oxide.

We think, therefore, it is very important to choose proper flux for its purpose. The flux should play a role excluding oxygen so that the oxygen can not touch the film where iron and zinc are sticked together. So far, various methods have been suggested to remove impurities on the surface of the material, keeping cleansing quality of the material just like foam of soap at the time of galvanization. With development of such product, we removed inconvenience which had been caused while using flux.

We have also been providing analysis of the Flux, managing the state of the liquid as well as supplying the Flux on the basis of actual record of performance and rich experience we have accumulated for a long time.

After that, we are devoting ourselves to the development of new Flux product to meet complex and diversified demand by using long experience and technology as a company specializing in making Flux.

1. List of KB Liquid Flux Product

Product
Type
Package
KB600
Liquid Flux for Wire Material
24kgs, 100kgs, 250kgs & Tank Lorry
KB700A
1:3 Mol ZnCl2 : NH4 Cl
"
KB700B
1:2 Mol ZnCl2 : NH4 Cl
"
KB700C
1:1 Mol ZnCl2 : NH4 Cl
"
KB800A
No Fume + C.G.L
"
KB800B
No Fly
"
KB800C
No Fume + No Fly
"
KB900
C.G.L
"
Special Liquid Flux
We develop it to comply with customers' demand

2. Characteristics of KB Fluid Flux

  1. It is easy to manage as its mol. ratio is stable.
  2. It is possible to cut down consumption amount of zinc as much as about 25%, compared with sole use of ammonium chloride.
  3. When dipped in a zinc tub, it has good protective effect because the surface to be galvanized increases in temperature and it is possible to decrease generation of dross.
  4. It increases luster of the surface of the coating and prevents pinholes from being generted.
  5. It gives the plating good adhesion and improves processing quality.
  6. It makes neutralized draining easy as it removes such harmful impurities as heavy metals
    (Please refer to below date)
Item
Measured Value
Item
Measured Value
Fe
Lower than 1.0ppm
Pb
Lower than 1.0ppm
Ni
Lower than 0.1ppm
Cr
Lower than 0.01ppm
Co
Lower than 0.1ppm
Cd
Lower than 0.01ppm
As
Lower than 0.1ppm
Cu
Lower than 0.1ppm

3. Standard of KB700 Flux

Name of Product
Zinc Chloride(ZnCl2)wt%
Ammonium Chloride(NH4Cl)wt%
1:3
46±3
54±3
1:2
56±3
44±3
1:1
72±3
28±3

4. Comparison of Performance of KB700 Fluid Flux

  • It is excellent in preventing zinc from flying during zinc bathing as well as removal of oxidized zinc and drying quality.
  • 1:! decreases fume while the object to be galvanized is dipped in a zinc tub thanks to the characteristics of Ammonium Chloride that is sublimated at the temperature of 330°C
Fume
Solidification
Heat-
resisting
quality
Removal of
oxidized zinc
Drying
quality
Flying
Zinc
Ash
1:3
O
O
O
O
O
O
1:1
O
X

5. Analysis and Management Service for KB Fluid Flux

  • Flux liquid is always managed so that it could be in a good state, as a result, defective products could be prevented and zinc consumption, dross and generation of zinc ash could be decreased; that is, the quality of the coating can be improved and the cost cut down.
  • We are contributing to the improvement of coating quality and cost cut-down by analyzing and evaluating flux liquid which is used.

6. KB Special Liquid Flux

We are also developing the following items, keeping up with advanced new plating technology in order to comply with complex and diversified demand.

  1. Fumeless flux
  2. Pre-treatment agent for plating
  3. Post-treatment agent for plating

*We are taking orders for special flux development to meet the users' demand.


PRODUCT : KB900. TYPE : C.G.L
Regarding KB900 Liquid Flux

1. Characteristics of the Liquid

  1. Specific Gravity : 1.2-1.4
  2. PH : 2.0-4.0
  3. Solute Content : More than 40%
  4. Color : Transparent Liquid
  5. Container : 250kg Plastic Drum

2. How to Use

  1. Working Temperature : 60C~80C
  2. Working Concentration : More than BE 30
    It shall be adjusted according to the used mehtod, byincreasing or decreasing.
  3. Tank Materials : Acid-resistance is recommended. The quality of the material from which iron is not eluted.
  4. Temperature Control : Indirect heating through a heat exchanger

3. Characteristics of KB900

  1. There is no interruption during working as it is mixed flux of complex composition with its main elements of chloride.
  2. It is excellent in removing the following impurities on the surface of the metal to be plated after pre-treatment.
    -Basic iron salt resulting fromiron salt being oxidized in the air when washing by water is not enough after acid pickling
    -Removal of Smut, reaction products after acid pickling.
    -Impurities like invisible oxide films.
  3. KB900 Flux removes oxide of melting metal on the bath surface when the metal to be plated is dipped into a zinc bath, as a result it can contact with clean material.
  4. It has excellent heat-resistance. It is non-inflammable at the atmosphere tetmperature of 1,000°C
  5. There is no occurrence of unplated portion as KB900 has high speed of separation when the metal to be plated is dipped into a zinc bath.

B2B Trade

Price (FOB) Negotiable transportation -
MOQ Negotiable Leadtime Negotiable
Payment Options Negotiable Shipping time Negotiable

KB ENG

Country / Year Established
South Korea South Korea /
Business type
Others

16

DUNS

President
Choi, Sung-suk
Address
237-11, Hakjang-dong, Sasang-gu, BUSAN, KOREA
Product Category
Other Chemicals
No. of Total Employees
501-1000
Company introduction

We have been acknowledged as the highest level in this business field with excellent human resources and experimental equipments on the basis of technology and experience we have accumulated for years.
Ouer research team manages quality control, improvement of quality, development of new products, receipt of request for development and enforcement and if necessary, analysis on the local situation.
As we ourselves produce raw materials, we can provide customers with the products at the minimum cost and therefore the price can be competitive. At present, 80% of flux for steel galvanization is provided by us in Korea. We also export flux for C.G.L. to Vietnam.
We are making effort to open a new market.

Main Markets

Viet Nam Viet Nam

Main Product

Related Products

Other buyers also search

Membership Grade

BUYER

Biz Pro VIP

SELLER

Biz Pro VIP
팝업닫기
Live Chat A new message arrives
from a business partner.

No Data

  • There is no data to load
  • Check out the My TK > My Inquiries list.
  • After agreeing to the use of the Live Chat service, the list is printed only when there is at least one history of receiving or sending a Live Chat request.

If you have not yet agreed to use the Live Chat service,

You can use the Live Chat freely after agreeing to the use of the Live Chat service.

View more
View more